Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

E-Polymers EFLEX® V2060 SEBS/TPV

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer E-Polymers Co. Ltd.
Trade Name EFLEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers EFLEX® V2060 SEBS/TPV.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
V-series (Thermoplastic Vulcanizate Resins): E-FLEX V series resins are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. E-FLEX V series resins are based on EPDM/PP or SEBS/SEEPS/PP(PE) utilizing new reactive grade polyolefins exhibiting high value/cost performance. It shows low temperature toughness, chemical resistance, ozone and UV resistant and wide service temperature range from -55 to 120°C for airbag covers, air dams, license plate holders and interior, as well as weather strip and exterior trim applications in automobile industry, for gasket in construction and appliance industry.Information Provided by E-Polymers Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 0.902 g/cc
0.902 g/cc
ASTM D792
Melt Flow 3.0 g/10 min

@Load 10.0 kg,
Temperature 230 °C
3.0 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
ASTM D2240
Tensile Strength 7.5537 MPa
1095.6 psi
ASTM D412
Elongation at Break 700 %
700 %
ASTM D412
Compression Set 20 %

@Temperature 23.0 °C
20 %

@Temperature 73.4 °F
ASTM D395
34 %

@Temperature 100 °C
34 %

@Temperature 212 °F
ASTM D395
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved