| Category | Polymer , Thermoplastic , Elastomer, TPE | 
| Manufacturer | Teknor Apex Company | 
| Trade Name | TELCAR® | 
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Teknor Apex Telcar® TL-1520C Thermoplastic Elastomer.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 | 
| Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | ASTM D955 | 
| Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ASTM D955 | 
| Melt Flow |           1.20           g/10 min           @Load 2.16 kg, Temperature 190 °C  | 
                  1.20           g/10 min           @Load 4.76 lb, Temperature 374 °F  | 
        ASTM D1238 | 
|           2.60           g/10 min           @Load 2.16 kg, Temperature 230 °C  | 
                  2.60           g/10 min           @Load 4.76 lb, Temperature 446 °F  | 
        ASTM D1238 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Shore A | 70 | 70 | ASTM D2240 | 
| Tensile Strength at Break | 9.17 MPa | 1330 psi | ASTM D412 | 
| Tensile Stress |           2.41           MPa           @Strain 100 %  | 
                  350           psi           @Strain 100 %  | 
        ASTM D412 | 
|           3.31           MPa           @Strain 300 %  | 
                  480           psi           @Strain 300 %  | 
        ASTM D412 | |
| Elongation at Break | 850 % | 850 % | ASTM D412 | 
| Tear Strength | 33.3 kN/m | 190 pli | Die C; ASTM D624 | 
| Compression Set |           31 %                     @Temperature 22.8 °C, Time 79200 sec  | 
                  31 %                     @Temperature 73.0 °F, Time 22.0 hour  | 
        ASTM D395B | 
|           81 %                     @Temperature 70.0 °C, Time 79200 sec  | 
                  81 %                     @Temperature 158 °F, Time 22.0 hour  | 
        ASTM D395B | |
|           90 %                     @Temperature 100 °C, Time 79200 sec  | 
                  90 %                     @Temperature 212 °F, Time 22.0 hour  | 
        ASTM D395B | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Dielectric Strength | 0.0984 kV/mm | 2.50 kV/in | ASTM D419 | 
| Processing Properties | Metric | English | Comments | 
|---|---|---|---|
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
| Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
| Front Barrel Temperature | 182 - 204 °C | 360 - 400 °F | |
| Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
| Zone 1 | 166 - 188 °C | 330 - 370 °F | |
| Zone 2 | 171 - 193 °C | 340 - 380 °F | |
| Zone 3 | 177 - 199 °C | 350 - 390 °F | |
| Zone 5 | 182 - 204 °C | 360 - 400 °F | |
| Die Temperature | 190 - 210 °C | 374 - 410 °F | |
| Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature | 
| Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
| Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
| Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Appearance | Opaque |