Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Parker Chomerics Tecknit Consil®-C 871 Silver-Copper Filled Silicone Elastomer

Category Polymer , Thermoset , Silicone
Manufacturer Parker Chomerics Tecknit
Trade Name Consil®-C
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics Tecknit Consil®-C 871 Silver-Copper Filled Silicone Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: CONSIL-C is a silicone or fluorosilicone elastomer filled with silver-plated copper particles designed to achieve maximum electrical conductivity. CONSIL-C provides one of the highest shielding effectiveness of any conductive elastomer material, in addition to offering excellent moisture sealing for all enclosure joints and seamTypical Applications: The MIL-DTL-83528 certified compounds meet the demanding requirements of many military and aerospace systems, and as gaskets for waveguides and connectors. In addition, CONSIL-C can also be used for EMP and TEMPEST applicationInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 3.045 - 3.955 g/cc
3.045 - 3.955 g/cc
ASTM D792
Deformation 10 %
10 %
10 pli; 0.125" diameter cord
10 %
10 %
39 pli; 0.125" by 0.25" strip
20 %
20 %
20 pli; 0.125" diameter cord
20 %
20 %
77 pli; 0.125" by 0.25" strip
Mechanical Properties Metric English Comments
Hardness, Shore A 58 - 72
58 - 72
ASTM D2240
Tensile Strength >= 1.38 MPa
>= 200 psi
ASTM D412
Elongation at Break 100 - 300 %
100 - 300 %
ASTM D412
Tear Strength 4.38 kN/m
25.0 pli
ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.0040 ohm-cm
<= 0.0040 ohm-cm
Shielding Effectiveness 75 dB

@Frequency 100000 Hz
75 dB

@Frequency 100000 Hz
H-Field
110 dB

@Frequency 1.00e+10 Hz
110 dB

@Frequency 1.00e+10 Hz
Plane Wave
115 dB

@Frequency 1.00e+9 Hz
115 dB

@Frequency 1.00e+9 Hz
Plane Wave
>= 120 dB

@Frequency 1.00e+7 Hz
>= 120 dB

@Frequency 1.00e+7 Hz
E-Field
Descriptive Properties Value Comments
Binder Silicone
Color Gray
Filler Silver Plated Copper Particles
Users viewing this material also viewed the following: