Material Notes:
BETABRACE™ 85076 is an expandable composite used for reinforcing sheet metal. It is composed of a high temperature curing tacky polymer, woven glass fabric, and release paper. BETABRACE™ 85076 provides adhesion to primed metal and also adheres to oily galvanized and cold rolled steel without a primer. BETABRACE™ 85076 can be supplied in many different shapes and thicknesses for specific reinforcement applications.Information provided by Dow
Thermal Properties Metric English Comments
Flash Point >= 204 °C
>= 400 °F
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 171 °C
0.167 hour

@Temperature 340 °F
Descriptive Properties Value Comments
Flexural Reinforcement Force N 30
2mm deflection; 1.3mm thick; After 500 hrs @ 200°F
33
2mm deflection; 1.9mm thick; After 500 hrs @ 200°F
35
2mm deflection; 1.3mm thick; After 500 hrs @ 100°F & 100% RH
40
2mm deflection; 1.3mm thick; Initial
40
2mm deflection; 1.3mm thick; After 14 days @ 190°F
45
2mm deflection; 1.9mm thick; After 500 hrs @ 100°F & 100% RH
57
2mm deflection; 1.9mm thick; Initial
57
2mm deflection; 1.9mm thick; After 14 days @ 190°F
Max Load N 155
1.3mm thick; 8mm max deflection
180
1.9mm thick; 7mm max deflection