Availability: North AmericaForms: PelletsFeatures: High Specific GravityInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 3.48 g/cc
0.126 lb/in³
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Thickness 3.17 mm
0.0020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Flexural Strength 48.3 MPa
7000 psi
ASTM D790
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm

@Thickness 3.17 mm
0.700 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 174 °C
345 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 167 °C
333 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.0 - 100 ohm-cm
1.0 - 100 ohm-cm
ASTM D257