Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sibur 21030 Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Sibur
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur 21030 Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Compounding for stabilization 16K, 16V, 16N, 16M, 16H superior quality. For production of technical and domestic products of complicated profile, of non-woven materials.
Physical Properties Metric English Comments
Melt Index of Compound 2.5 - 4.0 g/10 min
2.5 - 4.0 g/10 min
Ash <= 0.035 %
<= 0.035 %
For compounding of stabilization of 16M and painted marks are not normalized
Collected Volatile Condensable Material <= 0.090 %
<= 0.090 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 30.0 MPa
>= 4350 psi
Elongation at Break >= 500 %
>= 500 %
Descriptive Properties Value Comments
Mass Share of Isotactic Fraction Non-normalized
Number of Inclusions <3 pcs
Spread Flow Batch Error <±8 %
Users viewing this material also viewed the following: