Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 44.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Omni Plastics OmniTech™ ABS GP 12M
OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and ..
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Tensile Strength, Yield 44.8 MPa
6500 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Gravi-Tech™ GRV-NP-069-BMX Nylon 12  (discontinued **)
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Metton LMR M1539 Liquid Molding Resin
Metton LMR is a tough and durable engineering plastic material used to produce large or thick molded parts for many diversified applications. The Metton LMR reaction injection molding process can ..
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
M. Holland Company SA500 Styrene Acrylonitrile
High clarityGood processabilityHigh stiffnessApplications: Color concentratesCompounding
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Metton LMR M2100VO Liquid Molding Resin
Metton LMR is a tough and durable engineering plastic material used to produce large or thick molded parts for many diversified applications. The Metton LMR reaction injection molding process can ..
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Techmer ES Elastoblend® PA6 IM 835 HS L
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedProcessing Method: Injection MoldingInformat..
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Spartech Noryl® SP-5210 Specialty Sheet
Description: Specialty SheetNoryl is a registered trademark of General Electric Company.Information provided by Spartech.
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Techmer ES HiFill® PA6/6 0249 B Nylon 66
Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc.
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Techmer ES HiFill® PBT G/CF30 40% Glass Bead Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 40% Filler by WeightInformation provided by TP Composites, Inc.
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Techmer ES HiFill® POM 0223 B Acetal
Availability: North AmericaForms: PelletsFeatures: Copolymer and High Specific GravityInformation provided by TP Composites, Inc.
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Techmer ES Luriblend® PP GF20 GL2 BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Graphite Powder Lubricant(2%)Features: LubricatedAppearance: BlackInformation provided by TP..
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D 638
Styrolution PS 3100/3101 GPPS
Good balance of flow and set-up propertiesModerate heat resistanceUSP Class VI certifiedInformation provided by Styrolution
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM Data
Styron Magnumâ„¢ 2645 ABS, Impact Grade
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM Data
Styron Magnumâ„¢ 545 ABS, General Purpose
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM Data
Styron Magnumâ„¢ 780HP ABS, High Heat, High Impact
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Techmer ES HiFill® PA6 0254 B Barium Sulfate Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc.
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Techmer ES HiFill® PA6 0425
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityInformation provided by TP Composites, Inc.
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Techmer ES HiFill® TPU/E 0140
Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc.
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Techmer ES Luriblend® POM CO GM30 TL5 30% Glass Milled Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(5%)Features: Lubricated and CopolymerInformation provided by TP Compos..
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Westlake Plastics Dielux® PTFE filled Acetal Copolymer
Dielux PTFE filled acetal copolymer is an outstanding bearing and wear material for use in both wet and dry environments. It is frequently used in place of traditional metal and plastic bearing mat..
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Total PSC 536 Polystyrene
Polystyrene 536 is a high melt flow; high heat crystal polystyrene. Designed for fast cycle injection molding and for high output, direct injection profile extrusion for foam applications.Informatio..
Tensile Strength, Yield 44.8 MPa
6500 psi
chs 2 in/min; ASTM D638
Diamond Polymers ABS 3501
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Tensile Strength, Yield 44.8 MPa
6500 psi
chs 2 in/min; ASTM D638
Diamond Polymers ABS 3501 Natural 1050
Description: Natural, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Tensile Strength, Yield 44.8 MPa
6500 psi
chs 2 in/min; ASTM D638
Diamond Polymers ABS TS15v04 Injection Molding Grade, ABS/PC Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D-638
Axiall 7140 Rigid PVC, Extrusion & Molding
Georgia Gulf 7140 is a special purpose rigid PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChemical Resista..
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D-638
Axiall CL-6400 Rigid PVC, Molding
Georgia Gulf CL-6400 is a high flow clear PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of electrical and appliance applications.Information p..
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D-638
Axiall 7045 Rigid PVC, Extrusion
Georgia Gulf 7045 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityDimen..
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D-638
Axiall 8268 Rigid PVC, Extrusion
Georgia Gulf 8268 is a rigid PVC pellet compound suited for applications where transparency is important. It is widely used for clear profiles such as furniture trim, shower door and protected jalo..
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
PlastxWorld Veroplas PA2002HI Nylon 6
general purpose, unfilled, high impact modified injection molding gradeInformation provided by PlastxWorld Inc.