| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , PBT + PET Blend, Glass Filled , Polyethylene Terephthalate (PET) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Valox® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | SABIC Innovative Plastics Valox® 830F PBT+PET.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
| Density | 1.54 g/cc | 0.0556 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.0600 % | 0.0600 % | 23°C / 50% RH |
| 0.0600 % | 0.0600 % | 23°C / 50% RH; ISO 62 | |
| Water Absorption at Saturation | 0.15 % | 0.15 % | ASTM D570 |
| 0.15 % | 0.15 % | ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 18 g/10 min @Load 2.16 kg, Temperature 265 °C |
18 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D1238 |
| Melt Index of Compound | 13 g/10 min @Load 2.16 kg, Temperature 260 °C |
13 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 105 MPa | 15200 psi | Type I, 5 mm/min; ASTM D638 |
| 140 MPa | 20300 psi | 5 mm/min; ISO 527 | |
| Tensile Strength, Yield | 100 MPa | 14500 psi | Type I, 5 mm/min; ASTM D638 |
| 140 MPa | 20300 psi | 5 mm/min; ISO 527 | |
| Elongation at Break | 2.5 % | 2.5 % | Type I, 5 mm/min; ASTM D638 |
| 2.5 % | 2.5 % | 5 mm/min; ISO 527 | |
| Elongation at Yield | 2.5 % | 2.5 % | Type I, 5 mm/min; ASTM D638 |
| 2.5 % | 2.5 % | 5 mm/min; ISO 527 | |
| Tensile Modulus | 8.00 GPa | 1160 ksi | 5 mm/min; ASTM D638 |
| 9.00 GPa | 1310 ksi | 1 mm/min; ISO 527 | |
| Flexural Yield Strength | 170 MPa | 24700 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 200 MPa | 29000 psi | 2 mm/min; ISO 178 | |
| Flexural Modulus | 7.00 GPa | 1020 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 8.00 GPa | 1160 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
| 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
| 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| Dart Drop, Total Energy | 7.00 J @Temperature 23.0 °C |
5.16 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
13.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 25.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 81.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
45.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 202 °C | 396 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| 195 °C @Thickness 3.20 mm |
383 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 200 °C | 392 °F | Rate B/50; ASTM D1525 |
| 200 °C | 392 °F | Rate B/50; ISO 306 | |
| 205 °C | 401 °F | Rate B/120; ISO 306 |