Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.27 J/cm @Thickness 3.17 mm |
8.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Niche Polymer PCABSN8BK PC/ABS Information provided by Niche Polymer |
|||
Izod Impact, Unnotched | 4.27 J/cm @Temperature 22.8 °C |
8.00 ft-lb/in @Temperature 73.0 °F |
ASTM D4812 |
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced Polyetherimide, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Izod Impact, Unnotched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2300 PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification, KTW certification in recognized colors. |
|||
Izod Impact, Unnotched | 4.27 J/cm @Thickness 3.17 mm |
8.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrafil® J-1/CF/10 Nylon 66, 10% Carbon Fiber Reinforced |
|||
Izod Impact, Unnotched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DE0069F PC (Asia Pacific) LNP* Stat-kon* DE0069F is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, , Flame Retardant. |
|||
Izod Impact, Unnotched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP JF004EXP PES LNP* THERMOCOMP* JF004EXP is a compound based on Polyethersulfone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched | 4.27 J/cm @Temperature 23.0 °C |
8.00 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp KFI12A Acetal Homopolymer LNP LUBRICOMP* KFI12A is a compound based on Acetal Homopolymer resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABI.. |
|||
Izod Impact, Unnotched | 4.27 J/cm @Temperature 23.0 °C |
8.00 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem HU2410 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications.
Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Izod Impact, Unnotched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D4812 |
Asahi Kasei Thermofil P-20TC-1156 20% Talc Filled, Heat Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Unnotched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D4812 |
Asahi Kasei Thermofil P-20TC-1161 20% Talc Filled, Heat Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Unnotched | 4.27 J/cm | 8.00 ft-lb/in | 1/8 inch; ASTM D256 |
Adell ER-17 Homopolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |