SABIC Innovative Plastics Noryl EN130P PPE+PS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Noryl EN130P PPE+PS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High heat, extrusion grade PPO/HIPS alloy.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D 792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
Type I, 50 mm/min; ASTM D 638
Elongation at Break 30 %
30 %
Type I, 50 mm/min; ASTM D 638
Flexural Yield Strength 93.0 MPa
13500 psi
1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 2.00 GPa
290 ksi
1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 2.40 J/cm

@Temperature 23.0 °C
4.50 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 121 °C

@Thickness 3.20 mm
250 °F

@Thickness 0.126 in
unannealed; ASTM D 648
125 °C

@Thickness 6.40 mm
257 °F

@Thickness 0.252 in
unannealed; ASTM D 648