Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 170 °C | 338 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® FXM4701 PPC LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Americas .. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Asia Pacific) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Asia Pacific) XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Europe-Africa-Middle East) XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Vicat Softening Point | 170 °C | 338 °F | 49 N; ISO 306, ASTM D1525 |
Nilit Nilamid B3 H XB Unfilled, Impact Resistant PA6 Description: Nilamid B3 H XB is a high impact NYLON 6. The product has excellent impact properties above 0°C, combined with good maintaining mechanical characteristics. Application areas include au.. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® EXRL0627 PC Copolymer EXRL0627 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and transparent colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® FXM4701 PPC (Europe-Africa-Middle East) LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Europe-Af.. |
|||
Vicat Softening Point | 170 °C @Load 1.00 kg, Thickness 4.00 mm |
338 °F @Load 2.20 lb, Thickness 0.157 in |
ISO 306 |
Solvay Specialty Polymers Solef® 1015/0078 PVDF Homopolymer
(discontinued **) Key features of this grade: Plasticized, Offshore, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorina.. |
|||
Vicat Softening Point | 170 °C | 338 °F | 50 N; 50 °C/h; ISO 306 |
Lanxess Pocan® A 3122 901510 PBT+ASA, 20% Glass Fiber PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finishInformation provided by LANXESS. |
|||
Vicat Softening Point | 170 °C @Load 5.00 kg |
338 °F @Load 11.0 lb |
|
LATI Latamid 12 H2 G/30 PA 12, 30% Glass Fiber Reinforced, Heat Stabilized Polyamide 12 (PA12) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |
|||
Vicat Softening Point | 170 °C @Load 5.00 kg |
338 °F @Load 11.0 lb |
|
LATI Latigray 75/4-01 CX/45 PBT Radiopaque compound based on Polybutylene Terephthalate (PBT). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by L.. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WP004 is a compound based on Polybutylene Terephalate resin containing PTFE, Silicone. Added features include ; Internally Lubricated. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Ultem ATX100F PEI (Europe-Africa-Middle East) Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. US FDA Food Contact Compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Ultem HATX100 PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem HATX100 PEI+PCE (Europe-Africa-Middle East) Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate A/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ325HP PBT (Europe-Africa-Middle East) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate A/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® K3501 PBT Unfilled PBT, Hydrollytically Stable, Heat Stabilized, Impact Modified. A hydrollytically stable grade designed for improved performance under heat/humidity environments. Targeted at automotive unde.. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Asia Pacific) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Vicat Softening Point | 170 °C @Load 1.00 kg |
338 °F @Load 2.20 lb |
ASTM D1525 |
Eastman Eastman AP006 Copolyester Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly.. |
|||
Vicat Softening Point | 170 °C | 338 °F | 1kg load; ASTM D1525 |
Eastman Neostar FN005 Elastomer Neostar FN005 elastomer is a tough, clear, durable copolyester ether. It was designed for use in the profile and automotive markets, but is also used in packaging and tubing applications where tough.. |
|||
Vicat Softening Point | 170 °C | 338 °F | |
Covestro Apec® HT KU 1-9340 High-Heat Polycarbonate Transparent and opaque shades possible.Applications: Medical sector: superheated steam sterilization.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Ba.. |
|||
Vicat Softening Point | 170 °C | 338 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6000/42 Nylon 6, Polymer Modified, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 170 °C | 338 °F | 50°C/hr; 50N |
Arkema Group Rilsan® ASR 20 Nylon 12, 20% Carbon Fiber Filled (Conditioned) Designation ISO 1874-PA12,M,16-090,CF20Rigid grade with carbon fiber filler (20%) for injection molding. Available color: black. High strength-to-weight ratio. Very low shrinkage: include 0,5% on av.. |