Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 1.24 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
23/23°C; ASTM D792
RheTech Products G40P100-01 40% Glass Fiber Reinforced Polypropylene, Black
Injection molding conditions reported in table.Information provided by RheTech Products.
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
ASTM D792
S&E Specialty Polymers GA-1941-AFRO PVC
Application: 105° C PVC insulating compound designed for SJEOO applicationsInformation provided by S&E Specialty Polymers
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
NatureWorks® Ingeo™ 2003D General Purpose Transparent Extrusion Grade Biopolymer
NatureWorks® PLA polymer 2003D is a thermoplastic resin derived from annually renewable resources. PLA polymer 2003D processes easily on conventional extrusion equipment. Specifically designed fo..
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
NatureWorks® Ingeo™ 3001D Injection Grade PLA
NatureWorks® PLA (polylactide) polymer 3001D is designed for injection molding applications. It is designed for clear applications with heat deflection temperatures lower than 130ºF (55ºC). Appli..
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D1505
NatureWorks® Ingeo™ 4032D Film Grade PLA
NatureWorks® PLA (polylactide) polymer 4032D can be converted into a biaxially oriented film with use temperatures up to 300°F (150°C). This film has excellent optics, good machinability and exce..
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Polymer Resources PC-G10-IM Polycarbonate, 10% Glass Reinforced, Impact Modified
Polycarbonate, 10% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Specific Gravity 1.24 g/cc
1.24 g/cc
Radici Radilon® S RV200 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
SABIC Innovative Plastics LNP COLORCOMP G1000 PSU
LNP* COLORCOMP* G1000 is an unfilled Polysulfone resin. Added feature of this grade is: Transparent.
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU)  (Unverified Data**)
Udel P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion. Th..
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Solvay Specialty Polymers Udel® P-3700 HC Polysulfone (PSU)  (Unverified Data**)
Udel P-3700 HC is a high-clarity grade of polysulfone (PSU) that is nearly water-white in color. This grade was designed to eliminate the yellow cast and provide design flexibility and improved aest..
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Fiberfil® FPI-15 BK Nylon 6, 15% Glass Reinforced, post industrial
Information provided by FIBERFIL Engineered Plastics
Specific Gravity 1.24 g/cc
1.24 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 65-8285 PP-copolymer, with carbon fiber
Applications: Office communication.High-stiff parts with low creep.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided b..
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
ASTM D 792
Karina 722-48/1-A-IS Black PVC Compound
Heavy metal free PVC compound recommended for extrusion of automobile profilesInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
NBR NM-IEC 60811-1-3
Karina E 42/183-FC-LMP Red Color Concentrate for PVC
Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important con..
Specific Gravity 1.24 g/cc
1.24 g/cc
Sylvin Technologies 9600-85 Clear PVC Molding Compound
Information provided by Sylvin Technologies Inc.
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
SK Chemicals SKYTHANE® S155D Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Specific Gravity 1.24 g/cc
1.24 g/cc
23°C; ASTM D792
Teknor Apex Flexalloy® 9300-70 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, Oil Resistant, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather R..
Specific Gravity 1.24 g/cc
1.24 g/cc
23°C; ASTM D792
Teknor Apex MF 167 NT Polyvinyl Chloride, Flexible Film
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsAppearance-ClearAgency Ratings- USP Class VIInformation provided..
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Teknor Apex Sinvicomp SMG 4000 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Toys Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
A. Schulman POLYBATCH™ Weathered Wood 10418U Concentrate Based In LLDPE
DescriptionPOLYBATCH® Weathered Wood 10418U is a weathered wood color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide ..
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
A. Schulman POLYFORT™ FPP 1453 Calcium Carbonate Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1453 is a long term heat aging grade of 40% calcium carbonate filled homopolymer polypropylene. Information provided by A. Schulman.
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
A. Schulman POLYFORT™ FPP 1453 Calcium Carbonate Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1453 is a long term heat aging grade of 40% calcium carbonate filled homopolymer polypropylene. Information provided by A. Schulman.
Specific Gravity 1.24 g/cc
1.24 g/cc
Trelleborg B939 Nitrile Rubber
Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi..
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Lubrizol ESTANE® 58137 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Specific Gravity 1.24 g/cc
1.24 g/cc
ISO 2781
Lubrizol ESTANE® GP72DB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 72DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, TranslucentAvailable in EuropeInformati..
Specific Gravity 1.24 g/cc
1.24 g/cc
Colorite Polymers Self Frosting™ 8311SF Vinyl Compound
Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi..
Specific Gravity 1.24 - 1.28 g/cc
1.24 - 1.28 g/cc
ASTM D-792
Axiall 8651 Moldings & Extrusions Flexible PVC
A quality, low gravity extrusion compound with excellent low temperature properties. Designed for use in weatherstrips, flexible gaskets and extruded shapes.Information provided by Georgia GulfGeor..
Specific Gravity 1.24 g/cc
1.24 g/cc
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Hi-Sil 233 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Samyang Triel® 5652EM Thermoplastics Polyetherester Elastomer, Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5652EM is an extrusion grade.Information provided by Samyang.