Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

C.O.I.M. LARIPUR® LPR5925 Special Adipate Ester Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyester Thermoplastic Elastomer , Polyurethane, TP
Manufacturer C.O.I.M. S.p.A.
Trade Name Laripur®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF C.O.I.M. LARIPUR® LPR5925 Special Adipate Ester Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion resistanceGreat flexibility with constancy at temperature variationsGood compression resistanceGood water and light resistanceGood resistance to oils, fats and to many types of solventsSeries 25 Special Adipate Ester: These products are based on saturated polyesters. Products are based on saturated polyester. The features are similar to those of Series 20 but, by comparison, they are characterized by a higher resistance to hydrolysis and improved flexibility at low temperatures. Information provided by P.A.T. Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
ASTM D2240
Tensile Strength, Yield 68.9 MPa
9990 psi
ASTM D412
Elongation at Break 290 %
290 %
ASTM D412
50% Modulus 0.0164 GPa
2.38 ksi
ASTM D412
100% Modulus 0.0187 GPa
2.71 ksi
ASTM D412
300% Modulus 0.0450 GPa
6.53 ksi
ASTM D412
Flexural Modulus 0.235 GPa
34.1 ksi
ASTM D790
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -20.0 °C
2.38 ft-lb/in²

@Temperature -4.00 °F
ASTM D256
Tear Strength 171 kN/m
976 pli
ASTM D624
Abrasion 40
40
mm3, Abrasion Loss; DIN 53516
Torsional Stiffness 58.0 MPa
8410 psi
+20°C; ASTM D1043
370 MPa
53700 psi
-20°C; ASTM D1043
Thermal Properties Metric English Comments
Vicat Softening Point 146 °C
295 °F
ASTM D1525