| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® 503R PC
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release.
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® FL903 PC
Various weight reductions at 0.250"" (6.35 mm). High heat/creep resistance, excellent impact, flexural strength/rigidity. UV-stabilized.
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® FL920 PC
Various weight reductions at .250"" (6.35 mm) wall, 20% GR. Excellent flex mod, high tensile strength/heat resistance. V-0/5V at .250"" (6.35mm).
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® 953 PC
Opaque colors, high viscosity, superior flame retardance. UV-stabilized.
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® 953 PC (Asia Pacific)
Opaque colors, high viscosity, superior flame retardance. UV-stabilized.
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC 1 |
|
PTS Tristar® PC-20GFR 20% Glass Reinforced Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Asia Pacific)
Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA.
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® FL930 PC (Asia Pacific)
Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm).
|
|||
| Hot Wire Ignition, HWI |
60
-
120
sec <br>@Thickness 6.00 mm
|
60
-
120
sec <br>@Thickness 0.236 in
|
UL Rating PLC 1 (60-120 sec) |
|
Covestro Makrolon® SF-800 Polycarbonate, Structural Foam
(discontinued **)
Properties based on foam density of 0.90 g/cc.Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially..
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
|
SABIC Innovative Plastics Ultem 1010V PEI (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa..
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
|
SABIC Innovative Plastics ULTEM 1100 PEI (Asia Pacific)
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing.
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
|
SABIC Innovative Plastics Ultem 1100FV PEI
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th..
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
|
SABIC Innovative Plastics ULTEM 2100 PEI
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors.
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
|
SABIC Innovative Plastics ULTEM 2210 PEI (Asia Pacific)
20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
|
SABIC Innovative Plastics ULTEM 2210R PEI
20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
|
SABIC Innovative Plastics ULTEM 2210R PEI (Asia Pacific)
20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
|
SABIC Innovative Plastics Ultem 2313 PEI
30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region...
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
|
SABIC Innovative Plastics Ultem ATX100R PEI+PCE (Asia Pacific)
Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB listing.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
|
SABIC Innovative Plastics ULTEM HU1000 PEI (Asia Pacific)
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI)..
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
|
SABIC Innovative Plastics Ultem MD130A PEI
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
|
SABIC Innovative Plastics Valox® 420 PBT (Europe-Africa-Middle East)
VALOX 420 is a 30% glass fiber reinforced PBT injection moulding resin with excellent mechanical and thermal properties. Applications: appliance handles, spotlights, electric motors.
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
|
SABIC Innovative Plastics Valox® 553 PBT+PC (Asia Pacific)
30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc.
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
|
SABIC Innovative Plastics Valox® 553U PBT+PC
30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc.
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
|
SABIC Innovative Plastics Xenoy® 6370 PBT+PC
30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility.
|
|||
| Hot Wire Ignition, HWI |
60
-
120
sec <br>@Thickness 3.00 mm
|
60
-
120
sec <br>@Thickness 0.118 in
|
UL 746 |
|
Teknor Apex APEX® 1020 Polyvinyl Chloride, Semi-Rigid
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
|
|||
| Hot Wire Ignition, HWI |
60
-
119
sec <br>@Thickness 1.60 mm
|
60
-
119
sec <br>@Thickness 0.0630 in
|
UL PLC 1 (60-119 sec) |
|
Sumitomo Bakelite North America 73-70-70 C-P /73-70-70 VO-P Short-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I..
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
|
SABIC Innovative Plastics Noryl LS175 PPE+HIPS (Europe-Africa-Middle East)
Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del..
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
|
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PX5379 PPE+HIPS (Europe-Africa-Middle East)
LNP* Thermocomp* Noryl_PX5379 compound is a 10% GR. UL94 V-1 rated. Halogen free flame retardant. Typical applications are TV chassis, deflection yokes and connectors.
|
|||
| Hot Wire Ignition, HWI |
60
-
120
sec <br>@Thickness 3.00 mm
|
60
-
120
sec <br>@Thickness 0.118 in
|
UL 746 |
|
Teknor Apex APEX® 4011 Polyvinyl Chloride, Flexible
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
|
|||
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
|
SABIC Innovative Plastics NORYL RN0611 PPE+HIPS (Europe-Africa-Middle East)
Noryl RN0611 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen..
|
|||