Material Notes:
LNP* THERMOTUF* PX06093 is a compound based on PA 6 resin containing Impact Modifier. Added features include: High Impact, UV-Stabilized, Laser Marking Grade.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.019 - 0.021 cm/cm
0.019 - 0.021 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 50.0 MPa
>= 7250 psi
50 mm/min; ISO 527
Tensile Strength, Yield 45.0 MPa
6530 psi
50 mm/min; ISO 527
Flexural Yield Strength 56.0 MPa
8120 psi
2 mm/min; ISO 178
Flexural Modulus 1.50 GPa
218 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) >= 100 kJ/m²

@Temperature 23.0 °C
>= 47.6 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af