Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 100 kJ/m²

@Temperature -30.0 °C
47.6 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® 500RS PC (Europe-Africa-Middle East)
LEXAN 500RS is a medium viscosity, glass reinforced, flame retardant grade.
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® 513RS PC (Europe-Africa-Middle East)
LEXAN 513RS is a medium viscosity, glass reinforced, flame retardant grade UV stabilized grade.
Izod Impact, Unnotched (ISO) >= 100 kJ/m²

@Temperature -30.0 °C
>= 47.6 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® ML7686 PC (Europe-Africa-Middle East)
Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm.
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP FARADEX MS002 PP
LNP* FARADEX* MS002 is a compound based on Polypropylene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP FARADEX MS002 PP (Asia Pacific)
LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Izod Impact, Unnotched (ISO) 100 kJ/m²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Faradex MS002P PP (Asia Pacific)
LNP* Faradex* MS002P is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Exceptional Processi..
Izod Impact, Unnotched (ISO) 100 kJ/m² - NB
47.6 ft-lb/in² - NB
Average value: 109 kJ/m² Grade Count:6
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum ..
Izod Impact, Unnotched (ISO) 100 - 160 kJ/m²
47.6 - 76.1 ft-lb/in²
Average value: 120 kJ/m² Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an..
Izod Impact, Unnotched (ISO) 100 kJ/m² - NB
47.6 ft-lb/in² - NB
Average value: 117 kJ/m² Grade Count:3
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DL003E PC (Asia Pacific)
LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Easy Molding.
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP PFP36 PA 6
LNP* LUBRICOMP* PFL36 is a compound based on Nylon 6 resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant.
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP PFP36 PA 6 (Asia Pacific)
LNP* PFP36 is a compound based on Nylon 6 containing Glass Fiber and PTFE/Silicone. Characteristics are Impact Modifier.
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
ISO 180/1eU
Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, Conditioned
Description: TECHNYLSTAR Polyamide, reinforced with 50% of glass fiber, characterized by a high fluidity of the melt, for injection molding.Available in: Asia Pacific, Europe and North America Produ..
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
ISO 180/1eU
Solvay TECHNYLSTARâ„¢ SX 216 V60 PA6, 60% glass filled, Conditioned
Description: TECHNYL STAR TM Polyamide reinforced with 60% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North America Product Applicat..
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
ISO 180/1eU
Solvay TECHNYLSTARâ„¢ SX 218 L2 V60 Black JA6A PA6, 60% glass filled, Conditioned
Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, heat and UV stabilized, characterized by a high fluidity of the melt, for injection molding.Available in: Europe Product Applic..
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RFP36 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone.
Izod Impact, Unnotched (ISO) 100 kJ/m²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp ZP001 PPE+PS (Europe-Africa-Middle East)
LNP* LUBRICOMP* ZP001 is a compound based on PPE+PS Blend resin containing PTFE, Silicone. Added features include Internally Lubricated.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
Izod Impact, Unnotched (ISO) 100 kJ/m²

@Temperature -40.0 °C
47.6 ft-lb/in²

@Temperature -40.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Asia Pacific)
LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, ..
Izod Impact, Unnotched (ISO) >= 100 kJ/m²

@Temperature 23.0 °C
>= 47.6 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermotuf PX06093 PA 6 (Europe-Africa-Middle East)
LNP* THERMOTUF* PX06093 is a compound based on PA 6 resin containing Impact Modifier. Added features include: High Impact, UV-Stabilized, Laser Marking Grade.This data was supplied by SABIC-IP for t..
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON RV00AEXP PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00AEXP is a compound based on PA 66 resin containing Long Glass Fiber.
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
DIN 53453
Wico Plast Wicotal 500 Acetal
ApplicationsInjection moldingAll information provided by Wico Plast, Warenhandelsges. mbH
Izod Impact, Unnotched (ISO) >= 100 kJ/m²
>= 47.6 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Staramide PX06093 PA6, Impact Modified, Injection Molded
Staramide PX06093 is an UV Stabilized, Impact Modified Polyamide 6 Injection Molding Resin (also known as P1000HI020UVL)Information provided by Eurostar.
Izod Impact, Unnotched (ISO) 100 - 100 kJ/m²

@Temperature -30.0 - -30.0 °C
47.6 - 47.6 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 100 kJ/m² Grade Count:1
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
Izod Impact, Unnotched (ISO) >= 100 kJ/m²

@Temperature -30.0 - -30.0 °C
>= 47.6 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 100 kJ/m² Grade Count:1
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
DAM; ISO 180/1U
DuPont Performance Polymers Minlon® 12T BKB100 Nylon 66  (Unverified Data**)
36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T BKB100 is a 36% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe..
Izod Impact, Unnotched (ISO) 100 kJ/m²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermotuf PK003EI2 PA 6 (Europe-Africa-Middle East)
LNP* THERMOTUF* PK003EI2 is a compound based on PA 6 resin containing Impact Modifier, Mineral. Added features include High Impact, Easy Molding.This data was supplied by SABIC-IP for the Europe-Afr..
Izod Impact, Unnotched (ISO) 100 kJ/m²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Verton RV00CEU PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00CEU is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, UV Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON RV00CEXP PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00CE is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding.
Izod Impact, Unnotched (ISO) 100 kJ/m²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
80x10x4mm; ISO 180/1U
SYNTHOS Krasten® 562E High Impact Polystyrene
High impact grade with properties suitable for thermoforming. Processed mainly by extrusion and thermoforming. Production of plates, sheets, technical parts and molded packaging (used in e.g. the fo..
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics Xenoy® X5630P PET+PC (Europe-Africa-Middle East)
Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications