Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® 513RS PC (Europe-Africa-Middle East) LEXAN 513RS is a medium viscosity, glass reinforced, flame retardant grade UV stabilized grade. |
|||
Izod Impact, Unnotched (ISO) | >= 100 kJ/m² | >= 47.6 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® ML7686 PC (Europe-Africa-Middle East) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Izod Impact, Unnotched (ISO) | >= 100 kJ/m² @Temperature -30.0 °C |
>= 47.6 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® ML7686E PC (Europe-Africa-Middle East) Transparent Polycarbonate in natural color. Excellent processability, super high flow. UL compliant 94V-2 at 1.5mm. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX MS002 PP LNP* FARADEX* MS002 is a compound based on Polypropylene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Unnotched (ISO) | >= 100 kJ/m² | >= 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC (Europe-Africa-Middle East) LNP* Lubricomp* DL003 is a compound based on Polycarbonate resin containing PTFE. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² - NB | 47.6 ft-lb/in² - NB | Average value: 109 kJ/m² Grade Count:6 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1U |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN53G50HSLR BK083 is a 50% glass reinforced, heat stabilized, lubricated high performance polyamide resin developed for moderate temperature structural applications requiring retention of h.. |
|||
Izod Impact, Unnotched (ISO) | >= 100 kJ/m² | >= 47.6 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific) Transparent Polycarbonate in natural color. Excellent processability, super high flow. |
|||
Izod Impact, Unnotched (ISO) | >= 100 kJ/m² @Temperature -30.0 °C |
>= 47.6 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific) Transparent Polycarbonate in natural color. Excellent processability, super high flow. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² - NB | 47.6 ft-lb/in² - NB | Average value: 100 kJ/m² Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX MS002 PP (Europe-Africa-Middle East) LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | d.a.m.; ISO 180-1U |
Lanxess Durethan® B 30 S FN30 000000 Nylon 6, Flame Retardant PA 6, non-reinforced, injection molding, halogen free flame retardant, heat-aging resistanceInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DL003EU PC LNP LUBRICOMP* DL003EU is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, UV Stabilized, Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP PFP36 PA 6 (Asia Pacific) LNP* PFP36 is a compound based on Nylon 6 containing Glass Fiber and PTFE/Silicone. Characteristics are Impact Modifier. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | ISO 180/1eU |
Solvay TECHNYLSTARâ„¢ SX 218 L2 V60 Black JA6A PA6, 60% glass filled, Conditioned Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, heat and UV stabilized, characterized by a high fluidity of the melt, for injection molding.Available in: Europe Product Applic.. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFP36 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² @Temperature -30.0 °C |
47.6 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® 325FC PBT (Europe-Africa-Middle East) Commercial, VALOX 325FC is compliant with food contact regulations. VALOX 325FC is a general purpose, unreinforced PBT injection moulding resin which contains internal mold release. This new 325FC g.. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² @Temperature -40.0 °C |
47.6 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Europe-Africa-Middle East) LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Asia Pacific) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOTUF PK003ER PA 6 (Europe-Africa-Middle East) High Impact Nylon 6 compound containing Mineral, Impact Modifier. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RV00AEXP PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AEXP is a compound based on PA 66 resin containing Long Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | DIN 53453 |
Wico Plast Wicotal 500 Acetal ApplicationsInjection moldingAll information provided by Wico Plast, Warenhandelsges. mbH |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | ISO 180/1eU |
Lubrizol ESTALOC® T5160 Ether-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
Izod Impact, Unnotched (ISO) | 100 - 100 kJ/m² @Temperature -30.0 - -30.0 °C |
47.6 - 47.6 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 100 kJ/m² Grade Count:1 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermotuf PK003EI2 PA 6 (Europe-Africa-Middle East) LNP* THERMOTUF* PK003EI2 is a compound based on PA 6 resin containing Impact Modifier, Mineral. Added features include High Impact, Easy Molding.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RV00ASXS PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00ASXS is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Heat Stabilized |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RV00CEXP PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00CE is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm; ISO 180/1U |
SYNTHOS Krasten® 562E High Impact Polystyrene High impact grade with properties suitable for thermoforming. Processed mainly by extrusion and thermoforming. Production of plates, sheets, technical parts and molded packaging (used in e.g. the fo.. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Europe-Africa-Middle East) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Xenoy® X5630P PET+PC (Europe-Africa-Middle East) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |