SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* Stat-kon* SE003 is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 121 MPa
17500 psi
5 mm/min; ISO 527
Elongation at Break 2.8 %
2.8 %
5 mm/min; ISO 527
Tensile Modulus 8.60 GPa
1250 ksi
1 mm/min; ISO 527
Flexural Strength 172 MPa
24900 psi
2 mm/min; ISO 178
Flexural Modulus 7.60 GPa
1100 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 9.00 µm/m-°C

@Temperature 23.0 - 60.0 °C
5.00 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 156 µm/m-°C

@Temperature 23.0 - 60.0 °C
86.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 177 °C
351 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 167 °C
333 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 1000 ohm - 1e+05
1000 ohm - 1e+05
ASTM D257