Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Caplinq LINQSTAT™ VCF-40036S/2

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Caplinq
Trade Name LINQSTAT™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Caplinq LINQSTAT™ VCF-40036S/2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electronic, and Smartcard applications. Its easy-grounding nature makes it ideal for packaging where electrostatic contamination is a problem. The film and its conductivity are unaffected by humidity and age. The film is heat-sealable, flexible and offers exceptional abrasion resistance. Additionally, the film gives good thermal stability and has outstanding chemical resistance. The conductive bags meet electrical requirements of the military specification MIL-P-82646.Applications:Protection and storage of static-sensitive componentsInterleaf between rolls of Smartcard modulesGrounding MatsProduct Features and Benefits:Volume-conductive plasticBlack Opaque - PrintableProvides anti-static protection to electronic componentsGroundableHumidity indepentent conductivityChemical SusceptibilityMethanol: ResistantEthanol: ResistantIsopropanol: ResistantWeak Acids: ResistantKetones (Acetone): Slow AttackWeak Alkalines: Slow AttackHydrocarbons: Non-ResistantInformation provided by Caplinq
Physical Properties Metric English Comments
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.8 MPa
2000 psi
ASTM-D882
Film Elongation at Break, MD 330 %
330 %
ASTM-D882
Film Elongation at Break, TD 390 %
390 %
ASTM-D882
Dart Drop Test 380 - 400 g
0.838 - 0.882 lb
50% Failure Weight; ASTM D1709-67
Heat Seal Strength 3.00 - 9.23 g/25 mm
0.00661 - 0.0204 lb/in
Transverse Direction; ASTM-D882
3.51 - 10.8 g/25 mm
0.00774 - 0.0238 lb/in
Machine Direction; ASTM-D882
Electrical Properties Metric English Comments
Volume Resistivity <= 500 ohm-cm
<= 500 ohm-cm
ASTM-D991
Surface Resistivity per Square <= 31000 ohm
<= 31000 ohm
MIL 81705C
Static Decay <= 2.0 sec
<= 2.0 sec
EIA - Std 541