Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 261 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 127 °C

@Thickness 3.18 mm
261 °F

@Thickness 0.125 in
Annealed; ASTM D648
PolyOne Maxxam™ PPH-30T Nat Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ASTM D648
Network Polymers NPP 30-1200 TF20
Description: 20% Talc Filled Homopolymer PolypropyleneInformation provided by Network Polymers Inc.
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ASTM D648
Network Polymers NPP 30-2000 TF20
Description: 20% Talc Filled Homopolymer PolypropyleneInformation provided by Network Polymers Inc.
Deflection Temperature at 0.46 MPa (66 psi) 127 °C

@Thickness 3.20 mm
261 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® CH6310 PC+ABS (Asia Pacific)
CH6310 is a high heat, high flow PC/ABS resin, with nonbrominated, nonchlorinated flame retardant system. All color available.
Deflection Temperature at 0.46 MPa (66 psi) 127 °C

@Thickness 3.20 mm
261 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Asia Pacific)
CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.
Deflection Temperature at 0.46 MPa (66 psi) 127 °C

@Thickness 3.20 mm
261 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Lexan® EX7631T PC
EX7631T is a high UVA content homopolymer polycarbonate product intended for use as a cap layer for polycarbonate sheet extrusion.
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
Unannealed; ASTM Data
Dow Isoplast® 202 Polyurethane (PUR-RT), Impact Modified  (discontinued **)
ISOPLAST® 202 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include excellent chemical resistance, high heat, low mois..
Deflection Temperature at 0.46 MPa (66 psi) 127 °C

@Thickness 3.20 mm
261 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Valox® IQ357U PBT+PC
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ASTM D648
SPS Guang Zhou FILLMAâ„¢ 5002F30C Mineral Filled Polypropylene
Characteristic: 30%wt of Sulfate Calcium filled, low odor, good glossApplications: Household appliance parts, office suppliesInformation Provided by SPS (Guang Zhou) Ltd.
Deflection Temperature at 0.46 MPa (66 psi) 127 °C

@Thickness 6.40 mm
261 °F

@Thickness 0.252 in
ASTM D648
Samsung Cheil Industries Infino® HA-1011 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Deflection Temperature at 0.46 MPa (66 psi) 127 °C

@Thickness 6.40 mm
261 °F

@Thickness 0.252 in
ASTM D648
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ISO 75-1,-2
Topas Advanced Polymers TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC)
TOPAS® 5013L-10 is a high flow, internally lubricated injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, che..
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ISO 75-1,-2
Topas Advanced Polymers TOPAS® 5013S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 5013S-04 is a high flow injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high ..
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ASTM D648
Total PPH 3925WZ Polypropylene, Injection Molding Grade
Easy flow injection molding homopolymerNucleation - FINA 3925WZ is nucleated to provide fast cycle time and improve contact clarity.Antistat - FINA 3925WZ contains an antistat that will help protect..
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ASTM D648
Goodfellow TPX® RT31XB Injection Molding Grade Polymethylpentene
This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c..
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ASTM D648
Goodfellow TPX® DX845 Extrusion Grade Polymethylpentene
This grade is highly recommended for film extrusion; also for injection molding, fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensiv..
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ISO 75-1,-2
Covestro Bayblend® M850 XF PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Eas..
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ISO 75-1,-2
Covestro Bayblend® T80 XG PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Opt..
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ISO 75-1/-2
Covestro Bayblend® T85 Polycarbonate + ABS
General purpose injection molding gradeVicat/B 120 temperature = 131°Chigh impact and notched impact strengthPreprocessingMax. Water content
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ISO 75-1/-2
Covestro Bayblend® T85 XF Polycarbonate + ABS
General purpose injection molding gradeVicat/B 120 temperature = 130°Cbetter flow than T85PreprocessingMax. Water content
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ISO 75-1/-2
Covestro Bayblend® T90 MF-20* Polycarbonate + ABS, Mineral Filled
Developmental productInjection molding grade20 % mineral filledvery good flowreduced coefficient of thermal dilatationtensile modulus = 5200 MPaVicat/B 120 = 130 °CPreprocessingMax. Water content
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ASTM D648
Diamond Polymers NPP25-1602 TF40 40% Talc Filled Copolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ASTM D648
Diamond Polymers NPP30-0500 TF20 20% Talc Filled Homopolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ASTM D648
Ashley Polymers Ashlene® L925 Nylon 12
A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption. The natural c..
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
120°C/h; ISO 75/1
Polykemi AB POLYfill PPH T5040 FC VT Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP STAT-KON MFD02 PP
LNP* STAT-KON* MFD02 is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive.
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP STAT-KON MFD02 PP (Asia Pacific)
LNP* Stat-kon* MFD02 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
Polimeri Europa KOBLEND PCA 638 PC+ABS  (discontinued **)
Symbol according to ISO 1043/1: PC+ABS Injection moulding grade with very good impact behaviour even at low temperatures, good dimensional stability. Vicat/B50 = 120°C Main application fields: au..