| Category | Polymer , Thermoplastic , ASA Polymer | 
| Manufacturer | SABIC Innovative Plastics (GE Plastics) | 
| Trade Name | GELOY | 
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | SABIC Innovative Plastics GELOY HRA170 ASA (Europe-Africa-Middle East).pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 | 
| Moisture Absorption | 0.200 % | 0.200 % | 23°C / 50% RH; ISO 62 | 
| Water Absorption at Saturation | 0.60 % | 0.60 % | ISO 62 | 
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | on Tensile Bar; SABIC Method | 
| Melt Index of Compound |           17           g/10 min           @Load 5.00 kg, Temperature 260 °C  | 
                  17           g/10 min           @Load 11.0 lb, Temperature 500 °F  | 
        MVR [cm^3/10 min]; ISO 1133 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Rockwell R | 120 | 120 | ISO 2039-2 | 
| Hardness, H358/30 | 106 MPa | 15400 psi | ISO 2039-1 | 
| Tensile Strength at Break | 60.0 MPa | 8700 psi | 5 mm/min; ISO 527 | 
| 62.0 MPa | 8990 psi | 50 mm/min; ISO 527 | |
| Tensile Strength, Yield | 55.0 MPa | 7980 psi | 5 mm/min; ISO 527 | 
| 62.0 MPa | 8990 psi | 50 mm/min; ISO 527 | |
| Elongation at Break | >= 50 % | >= 50 % | 50 mm/min; ISO 527 | 
| 125 % | 125 % | 5 mm/min; ISO 527 | |
| Elongation at Yield | 4.0 % | 4.0 % | 50 mm/min; ISO 527 | 
| 5.0 % | 5.0 % | 5 mm/min; ISO 527 | |
| Tensile Modulus | 2.50 GPa | 363 ksi | 1 mm/min; ISO 527 | 
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 | 
| Flexural Modulus | 2.40 GPa | 348 ksi | 2 mm/min; ISO 178 | 
| Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1A | 
|           15.0           kJ/m²           @Temperature -30.0 °C  | 
                  7.14           ft-lb/in²           @Temperature -22.0 °F  | 
        80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA | 
|           1.20           J/cm²           @Temperature -30.0 °C  | 
                  5.71           ft-lb/in²           @Temperature -22.0 °F  | 
        Edgew 80*10*4 sp=62mm; ISO 179/1eA | |
| Taber Abrasion, mg/1000 Cycles | 95 | 95 | CS-17, 1 kg; SABIC Method | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| CTE, linear, Parallel to Flow |           80.0           µm/m-°C           @Temperature 23.0 - 60.0 °C  | 
                  44.4           µin/in-°F           @Temperature 73.4 - 140 °F  | 
        ISO 11359-2 | 
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 | 
| Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be | 
| Deflection Temperature at 1.8 MPa (264 psi) | 112 °C | 234 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae | 
| Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ISO 306 | 
| 132 °C | 270 °F | Rate B/120; ISO 306 | |
| Flammability, UL94 |           HB                     @Thickness 1.60 mm  | 
                  HB                     @Thickness 0.0630 in  | 
        UL 94 by SABIC-IP | 
| Oxygen Index | 22 % | 22 % | ISO 4589 | 
| Glow Wire Test |           750           °C           @Thickness 3.20 mm  | 
                  1380           °F           @Thickness 0.126 in  | 
        IEC 60695-2-12 | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 | 
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ROA; IEC 60093 | 
| Dielectric Constant |           2.8                     @Frequency 1.00e+6 Hz  | 
                  2.8                     @Frequency 1.00e+6 Hz  | 
        IEC 60250 | 
| Dielectric Strength |           17.0           kV/mm           @Thickness 3.20 mm  | 
                  432           kV/in           @Thickness 0.126 in  | 
        in oil; IEC 60243-1 | 
| Dissipation Factor |           0.013                     @Frequency 1.00e+6 Hz  | 
                  0.013                     @Frequency 1.00e+6 Hz  | 
        IEC 60250 | 
| Comparative Tracking Index | 225 V | 225 V | IEC 60112 | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Ball Pressure Test, 125°C +/- 2°C | PASSES | IEC 60695-10-2 |