Quadrant EPP Proteus® HDPE - High Density Polyethylene (ASTM Product Data Sheet)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Quadrant Engineering Plastics Products
Trade Name Proteus®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Proteus® HDPE - High Density Polyethylene (ASTM Product Data Sheet).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Natural and Black
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D792
Water Absorption <= 0.010 %
<= 0.010 %
Immersion, 24hr; ASTM D570(2)
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
ASTM D2240
Tensile Strength 31.7 MPa
4600 psi
ASTM D638
Elongation at Break 400 %
400 %
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Tensile Modulus 1.38 GPa
200 ksi
ASTM D638
Flexural Strength 31.7 MPa
4600 psi
ASTM D790
Flexural Modulus 1.20 GPa
174 ksi
ASTM D790
Compressive Strength 31.7 MPa
4600 psi
10% Def.; ASTM D695
Compressive Modulus 0.689 GPa
100 ksi
ASTM D695
Izod Impact, Notched 0.694 J/cm
1.30 ft-lb/in
ASTM D256 Type A
Coefficient of Friction, Dynamic 0.20
0.20
Dry vs. Steel; QTM55007
Thermal Properties Metric English Comments
CTE, linear 110 µm/m-°C

@Temperature -40.0 - 149 °C
61.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Melting Point 127 °C
260 °F
Crystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 82.2 °C
180 °F
Long Term
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ASTM D648
Flammability, UL94 HB
HB
1/8 inch (Estimated Rating)
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
ASTM D257
Surface Resistivity per Square >= 1.00e+15 ohm
>= 1.00e+15 ohm
ASTM D257
Compliance Properties Metric English Comments
3A-Dairy No
No
Canada AG No
No
FDA Yes
Yes
NSF No
No
USDA Yes
Yes
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Acceptable
Acceptable
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Unacceptable
Unacceptable
Conductive / Static Dissipative No
No
Continuous Sunlight Limited
Limited
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Unacceptable
Unacceptable
Hydrocarbons - Aromatic Unacceptable
Unacceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Unacceptable
Unacceptable
Descriptive Properties Value Comments
Machinability 3
1-10, 1=Easier to Machine