| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched |
0.694
J/cm <br>@Temperature 23.0 °C
|
1.30
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D256 |
|
RheTech Products FT4600-152 Thermoplastic Polyolefin, UV Stabilized, JA6A Black
Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
|
Nylene® NX4747 , 14% Glass Reinforced Translucent Nylon
Description: Nylene® NX4747 is a 14% glass fiber reinforced translucent specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of P..
|
|||
| Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
|
Ovation Polymers OPTRENE 20GF Polypropylene, 20% Glass Reinforced
Properties of chemically coupled glass reinforced (20%) polypropylene with high strength and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All ..
|
|||
| Izod Impact, Notched |
0.694
J/cm <br>@Temperature 22.8 °C
|
1.30
ft-lb/in <br>@Temperature 73.0 °F
|
ASTM D256 |
|
Polymer Resources PPX-MF-FRG20 Modified-PPO, 40% Glass/Mineral Reinforced, Flame Retardant
Modified-Polyphenylene Oxide, 40% Glass/Mineral Reinforced, Flame RetardantFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanica..
|
|||
| Izod Impact, Notched |
0.694
J/cm <br>@Thickness 3.18 mm
|
1.30
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
LNP Thermocomp® LF-1003 Polyetheretherketone, Glass Fiber Reinforcement
(discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
|
|||
| Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
|
M. Holland Company IS410 Polystyrene, High Impact
(discontinued **)
Features: Good Colorability, High Flow, Impact ModifiedUses: Household Goods, Modeling Material, ToysApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformation provided by M. Holl..
|
|||
| Izod Impact, Notched |
0.694
J/cm <br>@Thickness 3.17 mm
|
1.30
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Techmer ES Statiblend® ABS GF20 AS 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc.
|
|||
| Izod Impact, Notched |
0.694
J/cm <br>@Thickness 3.17 mm
|
1.30
ft-lb/in <br>@Thickness 0.125 in
|
injection molded sample; ASTM D256 |
|
American Polymers API 505 HF Polystyrene
API 505 HF is a high flow, intermediate grade of impact modified polystyrene. This material possess exceptional moldability and easy colorability. API 505 HF offers good retention of mechanical pr..
|
|||
| Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
|
Teknor Apex Synres® PP G10 17 Polypropylene, Glass Reinforced
Notes: The Specialty Compounding Division offers a proprietary line of glass reinforced polypropylene. Typical applications include automotive, building and construction, industrial as well as many ..
|
|||
| Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
|
A. Schulman ComAlloy® E-16558 30% Glass Fiber Reinforced Nylon
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Izod Impact, Notched |
0.694
J/cm <br>@Temperature 22.8 °C
|
1.30
ft-lb/in <br>@Temperature 73.0 °F
|
ASTM D256 |
|
Clariant 6618G15 HSL UV Black Nylon 66, 15% Glass Fiber, Impact Modified, UV and Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
|
Aclo Accutech ABS ABS831G30L Glass Reinforced |
|||
| Izod Impact, Notched |
0.694
J/cm <br>@Temperature -40.0 °C
|
1.30
ft-lb/in <br>@Temperature -40.0 °F
|
ASTM Test |
|
BASF Ultraform H 2320 006 Q600 POM
Ultraform H2320 006 is a high-molecular-weight grade of POM for injection molding. It conforms to FDA requirements of 21 CFR 177.2470.
|
|||
| Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
|
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength
(Unverified Data**)
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
|
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Izod Impact, Notched |
0.694
J/cm <br>@Temperature 23.0 °C
|
1.30
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D256 |
|
RheTech Products GC20P100-01 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
|
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry
(discontinued **)
Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg..
|
|||