Polymer Property : CTE, linear = 61.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 110 µm/m-°C

@Temperature -40.0 - 149 °C
61.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Proteus® HDPE - High Density Polyethylene (ASTM Product Data Sheet)
Natural and Black
CTE, linear 110 µm/m-°C

@Temperature -40.0 - 149 °C
61.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Sanalite® HDPE - High Density Polyethylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet)
CTE, linear 110 µm/m-°C

@Temperature -40.0 - 176 °C
61.0 µin/in-°F

@Temperature -40.0 - 349 °F
ASTM D696
Ravago Manufacturing Americas Hysun™ 693 ASA  (discontinued **)
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
CTE, linear 110 µm/m-°C

@Temperature 20.0 °C
61.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Westlake Plastics Ardel® Polyarylate
Stock shapes extruded from Ardel resin are specifically formulated to endure the damaging effects of UV light. When exposed to UV light, this unique material undergoes a molecular rearrangement res..
CTE, linear 110 µm/m-°C
61.0 µin/in-°F
ASTM D696
Ensinger Tecaform™ AH ID Metal Detectable Acetal Copolymer (POM)
TECAFORM™ AH ID is the fist commercially available acetal that is fully detectable by standard metal detection equipment. Exhibiting excellent machinability and a good combination of physical prop..