| Category | Ceramic , Oxide , Aluminum Oxide |
| Manufacturer | 3M |
| Trade Name | Nextel™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | 3M Nextel™ DF-11 Woven Fabric 610.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 3.90 g/cc | 0.141 lb/in³ | |
| Permeability | 20 | 20 | [ft<sup>3</sup>/min/ft<sup>2</sup>], Air w/o sizing |
| Thickness | 280 microns | 11.0 mil | |
| Fiber Count | 1670 dtex | 1500 denier | roving |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 3100 MPa | 450000 psi | filament 25.4mm |
| Tensile Modulus | 379 GPa | 55000 ksi | filament |
| Tear Strength | 40.2 kN/m | 230 pli | Warp, Breaking Strength w/o Sizing |
| 45.1 kN/m | 258 pli | Fill, Breaking Strength w/o Sizing |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 8.00 µm/m-°C @Temperature 100 - 1100 °C |
4.44 µin/in-°F @Temperature 212 - 2010 °F |
|
| Melting Point | 2000 °C | 3630 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.74 | 1.74 |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | 99 % | 99 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 9.0 @Frequency 9.375e+9 Hz |
9.0 @Frequency 9.375e+9 Hz |