Material Notes:
A general purpose injection molding ASA & ABS alloy. It has good mechanical properties similar to ABS with much better weather resistance.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ISO 2577
Melt Flow 15 g/10 min

@Load 2.10 kg,
Temperature 220 °C
15 g/10 min

@Load 4.63 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
ISO 527
Elongation at Break 90 %
90 %
ISO 527
Tensile Modulus 1.80 GPa
261 ksi
ISO 527
Flexural Strength 65.0 MPa
9430 psi
ISO 178
Flexural Modulus 2.00 GPa
290 ksi
ISO 178
Izod Impact, Notched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C
205 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093