Ascend Performance Materials Vydyne® 52BWMS Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® 52BWMS Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Vydyne® 52BWMS is a medium-viscosity resin used for extrusion-compounding. It is the product of choice for low-yellowness-required applications. This product with its higher viscosity is a part of 50BW/50BWFS series. It provides melt stability during the compound step to maintain its flow. Resistance of Vydyne 52BWMS to heat, oil and wear is typical of PA66 neat resins. Typical Applications/End Uses: CompoundingAvailability:Asia PacificEuropeNorth America Features: Gasoline ResistanceGeneral Purpose Good Chemical ResistanceGood Color StabilityOil ResistantSolvent ResistantUses:CompoundingGeneral Purpose Appearance: Natural ColorForms: PelletsProcessing Method: Compounding ExtrusionInformation provided by Ascend Performance Materials.
Physical Properties Metric English Comments
Bulk Density 0.674 g/cc
0.0243 lb/in³
ASTM D1895
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Moisture Absorption 0.350 %
0.350 %
ASTM D6869
Relative Viscosity 50 - 54 cP
50 - 54 cP
Formic Acid; ASTM D789
Viscosity Measurement 146 - 153
146 - 153
Viscosity Number cm³/g; H2SO4; ISO 307
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 11357-3
Optical Properties Metric English Comments
Yellow Index -4.00 %
-4.00 %
ASTM D1925