Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil LLDPE LL 5002.09 Linear Low Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Exxon Chemical
Trade Name LLDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LLDPE LL 5002.09 Linear Low Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: LL 5002.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. LL 5002.09 also exhibits good toughness and environmental stress crack resistance.Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoProcessing Aid: No Thermal Stabilizer: YesApplications: Masterbatch Base ResinInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ExxonMobil method
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 39

@Time 15.0 sec
39

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 13.1 MPa
1900 psi
ASTM D638
Tensile Strength, Yield 11.7 MPa
1700 psi
ASTM D638
Elongation at Break 730 %
730 %
ASTM D638
Flexural Modulus, 1% Secant 276 MPa
40000 psi
ASTM D638
Izod Impact, Notched 4.75 J/cm
8.90 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point <= 252 °C
<= 486 °F
Peak Melting Point; ExxonMobil method
Brittleness Temperature <= -76.1 °C
<= -105 °F
ASTM D746