Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M OFM0805 Outdoor UL Recognized Brite Silver Polyester Label Products

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M OFM0805 Outdoor UL Recognized Brite Silver Polyester Label Products.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Outdoor UL Recognized Brite Silver Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ Adhesive P1400 which is a high performance tackified acrylic designed for use in demanding environments.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Facestock
178 microns
7.00 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.386 kN/m
2.20 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 49.0 °C
120 °F
Application
150 °C
302 °F
Service
Minimum Service Temperature, Air -29.0 °C
-20.2 °F
Service
5.00 °C
41.0 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type P1400 Perm 21
Appearance 90# Polyctd.
Users viewing this material also viewed the following: