Hexcel® HexPly® 913 125°C Curing Epoxy Matrix

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® 913 125°C Curing Epoxy Matrix.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HexPly® 913 is a proven modified epoxy matrix with a low temperature cure cycle which exhibits outstanding environmental resistance, whilst retaining good hot/wet mechanical performance. This versatile matrix system can be processed using a wide range of techniques according to the application and is capable of co cure with epoxy film adhesives.HexPly® 913 is a highly successful matrix used extensively in the aerospace industry for primary aircraft structures and helicopter blades.Features: Exceptional environmental resistance, Controlled minimum viscosity giving easy processing, Capable of being processed by various techniques, Good tack and drape characterisitics, Long shelf life and out life at room temperature, Compatible with Redux 312 and 335K adhesive films
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
Cured
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.5 MPa
9500 psi
ISO R527 type 1
Tensile Modulus 3.39 GPa
492 ksi
ISO R527 type 1