| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Geon™ Vinyl Flexible A4DU5 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.26 g/cc | 1.26 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 86 | 86 | 15 sec; ASTM D2240 |
| 93 | 93 | ASTM D2240 | |
| Hardness, Shore D | 40 | 40 | 15 sec; ASTM D2240 |
| 53 | 53 | ASTM D2240 | |
| Tensile Strength at Break | 20.0 MPa | 2900 psi | 510 mm/min; ASTM D638 |
| Tensile Strength | 14.5 MPa @Strain 100 % |
2100 psi @Strain 100 % |
510 mm/min; ASTM D638 |
| Elongation at Break | 330 % | 330 % | 510 mm/min; ASTM D638 |
| Tear Strength | 114 kN/m | 650 pli | Die C, 510 mm/min; ASTM D624 |
| Compression Set | 60 % @Temperature 23.0 °C, Time 79200 sec |
60 % @Temperature 73.4 °F, Time 22.0 hour |
ASTM D395 |
| Clash Berg Modulus | 0.758 GPa | 110 ksi | ASTM D1043 |
| 0.310 GPa @Temperature -13.0 °C |
45.0 ksi @Temperature 8.60 °F |
ASTM D1043 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 177 - 188 °C | 351 - 370 °F | |
| 193 - 204 °C | 379 - 399 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Clear/Transparent | |
| Features | General Purpose | |
| Good UV Resistance | ||
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | General Purpose |