Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CoorsTek AIN-170 Hot Pressed Aluminum Nitride

Category Ceramic , Nitride
Manufacturer CoorsTek
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CoorsTek AIN-170 Hot Pressed Aluminum Nitride.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Aluminum Nitride Advantages: High heat dissipation with thermal conductivity of 170 W/m K Non-toxic alternative to BeO Thermal expansion coefficient similar to Si, GaN, and GaAs semiconductors High dielectric strengthInformation provided by CoorsTek, Inc.
Physical Properties Metric English Comments
Density 3.31 g/cc
0.120 lb/in³
ASTM C373
Mechanical Properties Metric English Comments
Flexural Strength >= 350 MPa
>= 50800 psi
ASTM F417
Thermal Properties Metric English Comments
CTE, linear 4.20 µm/m-°C

@Temperature 25.0 - 1000 °C
2.33 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
Thermal Conductivity >= 170 W/m-K
>= 1180 BTU-in/hr-ft²-°F
ASTM E1461
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm

@Temperature 25.0 °C
>= 1.00e+13 ohm-cm

@Temperature 77.0 °F
ASTM D257
Dielectric Constant 8.0

@Frequency 1.00e+6 Hz
8.0

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength >= 15.0 kV/mm

@Thickness 0.635 mm
>= 381 kV/in

@Thickness 0.0250 in
ASTM D149
Dissipation Factor 0.00020
0.00020
Dielectric Loss Index 0.0016

@Frequency 1.00e+6 Hz
0.0016

@Frequency 1.00e+6 Hz
ASTM D150
Descriptive Properties Value Comments
Surface Finish As-fired (Ra) (micron) <0.5
Profilometer 5.08µmicron Radius Stylus; 2,540 µmicron Cutoff ANSI/ASME B46.1