| Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
| Manufacturer | PolyOne Corporation |
| Trade Name | Bergamid™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Bergamid™ B70 W25 Polyamide 6 (Nylon 6).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.10 g/cc | 0.0397 lb/in³ | ±0.03 g/cm³; DIN 53479 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 70.0 MPa | 10200 psi | ISO 527-2 |
| Elongation at Break | 4.0 % | 4.0 % | ISO 527-2 |
| Tensile Modulus | 2.90 GPa | 421 ksi | ISO 527-2 |
| Charpy Impact Unnotched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ISO 179 |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
ISO 179 | |
| Charpy Impact, Notched | 0.900 J/cm² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
| 1.50 J/cm² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 223 °C | 433 °F | |
| Maximum Service Temperature, Air | 65.0 °C | 149 °F | Continuous (GTP 50% Tensile) |
| 160 °C | 320 °F | Short Time | |
| Deflection Temperature at 0.46 MPa (66 psi) | 170 °C | 338 °F | Unannealed; ISO 75-2/B |
| Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | Unannealed; ISO 75-2/A |
| Flammability, UL94 | HB @Thickness 0.800 mm |
HB @Thickness 0.0315 in |
UL 94 |
| HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
| Dielectric Constant | 3.4 @Frequency 1.00e+6 Hz |
3.4 @Frequency 1.00e+6 Hz |
IEC 60250 |
| Dielectric Strength | 100 kV/mm | 2540 kV/in | IEC 60243-1 |
| Dissipation Factor | 0.20 @Frequency 1.00e+6 Hz |
0.20 @Frequency 1.00e+6 Hz |
IEC 60250 |
| Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | Impact Modified | |
| Forms | Pellets | |
| Generic Material | Nylon 6 | |
| Generic Name | Polyamide 6 (Nylon 6) | |
| Regional Availability | Europe | |
| RoHS Compliance | RoHS Compliant |