Plastcom SLOVAMID 6 GF 7 T 13 PA6, 7% glass fibre, 13% mineral filling

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVAMID 6
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVAMID 6 GF 7 T 13 PA6, 7% glass fibre, 13% mineral filling.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesGood anisotropy of the manufacturing shrinkage. The talc is added to get the material shrinkage identical in both directions. Application for flat products in disc form /no screw after cooling off/ and for thick-walled products, at which the protection against the material failure is guaranteed. PA for injection moulding with the content of 13% micromilled talc. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
Viscosity Measurement 0.93 - 1.12
0.93 - 1.12
Linear Mold Shrinkage 0.0093 cm/cm
0.0093 in/in
Linear Mold Shrinkage, Transverse 0.0112 cm/cm
0.0112 in/in
Melt Flow 8.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
8.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 95.0 MPa
13800 psi
Elongation at Break 5.0 %
5.0 %
Tensile Modulus 4.80 GPa
696 ksi
Flexural Strength 165 MPa
23900 psi
Flexural Modulus 4.55 GPa
660 ksi
Charpy Impact Unnotched 4.00 J/cm²

@Temperature -20.0 °C
19.0 ft-lb/in²

@Temperature -4.00 °F
4.50 J/cm²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.400 J/cm²

@Temperature -20.0 °C
1.90 ft-lb/in²

@Temperature -4.00 °F
0.600 J/cm²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
Vicat Softening Point 210 °C
410 °F
B
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Melt Temperature 240 - 270 °C
464 - 518 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Moisture Content 0.15 %
0.15 %
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi