Material Notes:
FeaturesPA 6 for injection moulding with increased flammability resistance. Halogen-free flame retardant. Intended for electrical purposes. Manufacturing of simple large scale products. Good flow, good resistance against injection failure. Suitable also for thin-walled products, large scale cable boxes. Delivered in natural and in the full RAL color scale.Application: Injection MouldingInformation Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
STN 64 0111
Linear Mold Shrinkage 0.0147 cm/cm
0.0147 in/in
STN 64 0808
Linear Mold Shrinkage, Transverse 0.0153 cm/cm
0.0153 in/in
STN 64 0808
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
STN EN ISO 527-2
Elongation at Break 4.0 %
4.0 %
STN EN ISO 527-2
Tensile Modulus 2.80 GPa
406 ksi
STN EN ISO 527-2
Flexural Strength 95.0 MPa
13800 psi
STN EN ISO 178
Flexural Modulus 3.00 GPa
435 ksi
STN EN ISO 178
Charpy Impact Unnotched 5.00 J/cm²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
5.00 J/cm²

@Temperature -20.0 °C
23.8 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Charpy Impact, Notched 0.200 J/cm²

@Temperature -20.0 °C
0.952 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
0.300 J/cm²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
DSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
STN EN ISO 75/A
Vicat Softening Point 200 °C
392 °F
B; STN EN ISO 306
Flammability, UL94 V-0
V-0
Glow Wire Test 960 °C
1760 °F
STN IEC 60695-2-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
STN IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
STN IEC 60093
Dielectric Strength 20.0 kV/mm
508 kV/in
STN IEC 60243
Comparative Tracking Index 500 V
500 V
STN 34 6468
Processing Properties Metric English Comments
Melt Temperature 250 - 270 °C
482 - 518 °F
Mold Temperature 50.0 - 70.0 °C
122 - 158 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Moisture Content 0.15 %
0.15 %
STN EN ISO 960
Injection Pressure 70.0 - 100 MPa
10200 - 14500 psi