Material Notes:
PERMABOND TA4810 is a 2-part, 1:1 toughened methacrylate adhesive designed for bonding thermoplastics, thermosets, metals and composites.  TA4810 has excellent adhesion to as received metal surfaces forming high strength bonds without surface preparation. It provides excellent durability and resistance to many common industrial solvents, fuels as well as environmental conditions. It cures rapidly at room temperature and has very good thixotropic properties allowing for easy dispensing through static mixers while maintaining good gap filling and non-sag properties. Features & Benefits: Adhesion to a wide variety of substrates Fast cure at room temperature High shear and peel strength Good impact strength Good chemical resistance Information provided by Permabond.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
TA4810A
1.04 g/cc
0.0376 lb/in³
TA4810B
Viscosity 40000 - 60000 cP

@Temperature 25.0 °C
40000 - 60000 cP

@Temperature 77.0 °F
TA4592A
40000 - 60000 cP

@Temperature 25.0 °C
40000 - 60000 cP

@Temperature 77.0 °F
TA4592B
90000 - 100000 cP

@Temperature 25.0 °C
90000 - 100000 cP

@Temperature 77.0 °F
Mixed Viscosity
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Tensile Strength 28.938 MPa
4197.1 psi
DIN 53283
Elongation at Break 15 - 20 %
15 - 20 %
Adhesive Bond Strength >= 11.7 MPa
>= 1700 psi
Fiber glass, Shear; ASTM D1002
20.67 - 27.56 MPa
2998 - 3997 psi
Aluminum, Shear; ASTM D1002
24.1 - 31.0 MPa
3500 - 4500 psi
Steel, Shear; ASTM D1002
Peel Strength 2.625 - 3.50 kN/m
14.98 - 20.0 pli
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C
44.4 µin/in-°F
ASTM D696
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
ASTM C177
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Dielectric Constant 4.6

@Frequency 1.00e+7 Hz
4.6

@Frequency 1.00e+7 Hz
ASTM D150
Dielectric Strength 30.0 - 50.0 kV/mm
762 - 1270 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 4.02 - 6.00 min
0.0670 - 0.100 hour
working strength
10.0 - 15.0 min
0.167 - 0.250 hour
fixture time
1440 min
24.0 hour
full cure
Shelf Life 6.00 Month
6.00 Month
12.0 Month
12.0 Month
refrigerated
Descriptive Properties Value Comments
Appearance Amber, TA4810B
Uncured
Off-white, TA4810A
Uncured
Maximum Gap Fill (mm) 2
Strength Retention 10% at 200°C
Relative to 0°C
100% at 0°C
Relative to 0°C
30% at 150°C
Relative to 0°C
75% at 100°C
Relative to 0°C
96% at 50°C
Relative to 0°C