Dow Corning SILASTIC® 3496 MOULD MAKING BASE & 96 CURING AGENT

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® 3496 MOULD MAKING BASE & 96 CURING AGENT.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High strength, low hardness, fast cure silicone mold making rubber featuring a very good resistance to polyester resin and suited for the detailed reproduction of fiines, art objects and similar items.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc

@Temperature 25.0 °C
1.14 g/cc

@Temperature 77.0 °F
Viscosity 11200 cP
11200 cP
mixing, dynamic
Mechanical Properties Metric English Comments
Hardness, Shore A 10
10
Tensile Strength, Ultimate 2.96 MPa
430 psi
Elongation at Break 490 %
490 %
Tear Strength 21.0 kN/m
120 pli
Descriptive Properties Value Comments
Mix Ratio (X:1) 10
Working Time (min) 120