Material Notes:
Permabond® HH120 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking bolts, nuts and screws that require permanent assembly. Its high viscosity allows for ease of use on coarse threaded fasteners. Cure is fast and reliable on steel, cadmium, zinc and other plated fasteners. Major use areas include machinery and equipment manufacturing. Additional uses include sealing pipe flanges and retaining worn bearings. Features & Benefits: Prevents vibration loosening Controlled off-torque Non-drip, thixotropic Full cure at room temperature Provides corrosion protection Superior environmental resistance Environmentally friendly – 100% solids Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Viscosity 7000 cP

@Temperature 25.0 °C
7000 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Adhesive Bond Strength 17.0 MPa
2470 psi
steel collar and pin shear; ISO 10123
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 11.0 kV/mm
279 kV/in
Processing Properties Metric English Comments
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
10.2 min

@Temperature 23.0 °C
0.170 hour

@Temperature 73.4 °F
M10 steel, handling strength
15.0 min

@Temperature 23.0 °C
0.250 hour

@Temperature 73.4 °F
Brass, working strength
30.0 min

@Temperature 23.0 °C
0.500 hour

@Temperature 73.4 °F
Zinc, handling strength
30.0 min

@Temperature 23.0 °C
0.500 hour

@Temperature 73.4 °F
M10 steel, working strength
360 min

@Temperature 23.0 °C
6.00 hour

@Temperature 73.4 °F
Stainless steel, handling strength
1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
Zinc, working strength
1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
M10 steel, full strength
Descriptive Properties Value Comments
Appearance Red
Uncured
Maximum Gap Fill (mm) 0.25
Maximum Thread Size M30
Strength Retention 50% at 150°C
Relative to 0°C
80% at 100°C
Relative to 0°C
93% at 50°C
Relative to 0°C
Torque Strength (N m) 31
M10 steel, break
34
M10 steel, prevail
UV Fluorescence Yes
Uncured