| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced |
| Manufacturer | Aclo Compounders |
| Trade Name | Accutech |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Aclo Accutech Polypropylene Copolymer CP0436W20L Wollastonite Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0080 cm/cm | 0.0080 in/in | MD; ASTM D955 |
| Melt Flow | 11 g/10 min | 11 g/10 min | ASTM D1238 |
| Ash | 20 % | 20 % | ASTM D2584 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 55 | 55 | ASTM D785 |
| Tensile Strength at Break | 16.0 MPa | 2320 psi | ASTM D638 |
| Tensile Strength, Yield | 21.0 MPa | 3050 psi | ASTM D638 |
| Elongation at Break | 26 % | 26 % | ASTM D638 |
| Elongation at Yield | 5.0 % | 5.0 % | ASTM D638 |
| Tensile Modulus | 1.700 GPa | 246.5 ksi | ASTM D638 |
| Flexural Strength | 25.0 MPa | 3630 psi | ASTM D790 |
| Flexural Modulus | 1.450 GPa | 210.3 ksi | ASTM D790 |
| Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 109 °C | 228 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 56.1 °C | 133 °F |