| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
Nilit Polynil® N66-P300 High Viscosity Nylon 6/6
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
Nilit Polynil® N66-P50N Lubed Nylon 6/6
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
PTS Trimid® N66-100HL Heat Stabilized, Lubed Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
PTS Trimid® N66-100L Lubed Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
PTS Trimid® N66-100NL Nucleated, Lubricated Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
PTS Trimid® N66-1010 Utility Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
PTS Trimid® N66-1010L Lubed, Utility Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
PTS Trimid® N66-G13 13% Glass Fiber Reinforced Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
PTS Trimid® N66-G13HL 13% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
PTS Trimid® N66-G13L 13% Glass Fiber Reinforced Lubed Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
PTS Trimid® N66-G33 33% Glass Fiber Reinforced Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
PTS Trimid® N66-G33HL 33% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
PTS Trimid® N66-G33L 33% Glass Fiber Reinforced Lubed Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
PTS Trimid® N66-G43HL 43% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
PTS Trimid® N66-G43L 43% Glass Fiber Reinforced Lubricated Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
PTS Trimid® N66-S100HL-BK High Impact Heat Stabilized Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
PTS Trimid® N66-SG33-BK 33% Glass Reinforced, High Impact Black Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
PTS Trimid® N66-T100 Toughened Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
PTS Trimid® N66-T100HL Toughened, Heat Stabilized, Lubed Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
PTS Trimid® N66-G13LU 13% Glass Fiber Reinforced Utility Lubricated Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
PTS Trimid® N66-S100L High Impact Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||