Polymer Property : Flexural Yield Strength = 68.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Ravago Manufacturing Americas Hybrid S459 ABS + Polycarbonate Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Flexural Yield Strength 68.9 - 147 MPa
10000 - 21300 psi
Average value: 109 MPa Grade Count:35
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Flexural Yield Strength 68.9 - 181 MPa
10000 - 26300 psi
Average value: 104 MPa Grade Count:28
Overview of materials for Acetal Copolymer, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values ..
Flexural Yield Strength 68.9 - 200 MPa
10000 - 29000 psi
Average value: 120 MPa Grade Count:19
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim..
Flexural Yield Strength 68.9 - 179 MPa
10000 - 26000 psi
Average value: 91.2 MPa Grade Count:63
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
Flexural Yield Strength 68.9 - 133 MPa
10000 - 19300 psi
Average value: 103 MPa Grade Count:15
Overview of materials for Acrylic, Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o..
Flexural Yield Strength 68.9 - 260 MPa
10000 - 37700 psi
Average value: 139 MPa Grade Count:37
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% ..
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Spartech CamAlloy /ABS Weatherable Sheet
Description: Weatherable SheetInformation provided by Spartech.
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Spartech Panel Pro ABS UV-Resistant Embossed Sheet Specialty Sheet
Description: Specialty SheetInformation provided by Spartech.
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Spartech Soft Touch ASA/ABS Co-Extruded Specialty Sheet
Description: Specialty SheetInformation provided by Spartech.
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Spartech SP-9070 ABS/PVC Flame Retardant Sheet
Description: Flame Retardant SheetInformation provided by Spartech.
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Star Plastics ABS9020 Molding Grade ABS
Information provided by Star Plastics, Inc.
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Star Plastics ABSLG3030 Molding Grade ABS, Low Gloss
Information provided by Star Plastics, Inc.
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Star Plastics PC/ABSQX7005 Molding Grade PC/ABS
Information provided by Star Plastics, Inc.
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Techmer ES HiFill® PP GF10 CC 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc.
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Star Plastics ABS3545 Molding Grade ABS
Information provided by Star Plastics, Inc.
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
PlastxWorld CEVIAN® SER91 ABS
General purpose and flame retarded ABS with excellent moldability and no plate-out.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Informat..
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
PlastxWorld CEVIAN®-V 660SF ABS
High Flow ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Westlake Plastics Dielux® PTFE filled Acetal Copolymer
Dielux PTFE filled acetal copolymer is an outstanding bearing and wear material for use in both wet and dry environments. It is frequently used in place of traditional metal and plastic bearing mat..
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Formosa Plastics Formolon® APW Compound
APW Powder Window Profile Compound Series The APW compounds have been designed for profile extrusion in window lineals, fencing and other outdoor weatherable markets. It exhibits excellent whiteness..
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Formosa Plastics Formolon® AWS Compound
AWS Powder Profiler Compound Series The AWS compounds have been designed for profile extrusion in indoor and non-weatherable applications and substrates for outdoor applications. They exhibit a natu..
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Clariant 6604-HSL Nylon 66, Impact Modified, Heat Stabilized
Data provided by Clariant Masterbatches
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Clariant Renol PBT1700 Polybutylene Terephthalate, Flame Retardant
Data provided by Clariant Masterbatches
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Clariant Renol PCSP0007 Polycarbonate/Polyester Alloy
Data provided by Clariant Masterbatches
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Clariant Renol PCSP0016BL-201 Polycarbonate/Polyester Alloy
Data provided by Clariant Masterbatches
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Techmer ES HiFill® TPU GF30 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc.