Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mytex Polymers AS65KW-1ATM Polypropylene, Talc filled, Compounded

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Talc Filler
Manufacturer Mytex Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mytex Polymers AS65KW-1ATM Polypropylene, Talc filled, Compounded.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: Non-painted instrument panelInformation provided by Mytex Polymers
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Melt Flow 19 g/10 min
19 g/10 min
ASTM D1238
Ash 23 %
23 %
ASTM D5630
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
Instant; ASTM D648
Tensile Strength, Yield 23.0 MPa
3340 psi
50 mm/min; ASTM D638
Flexural Modulus 2.45 GPa
355 ksi
Tangent; 1.3 mm/min; ASTM D790
Izod Impact, Notched 4.50 J/cm

@Temperature 23.0 °C
8.43 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
ASTM D648