Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Nylex™ 1230 Natural Polyamide + PP

Category Polymer , Thermoplastic , Nylon , Polypropylene (PP)
Manufacturer Multibase
Trade Name Nylex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Nylex™ 1230 Natural Polyamide + PP.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing, Electrical Safety EquipmentInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM 792
Water Absorption 0.65 %
0.65 %
ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Melt Flow 0.95 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.95 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 21.0 MPa
3050 psi
ASTM D638
Elongation at Break 160 %
160 %
ASTM D638
Flexural Strength 20.7 MPa
3000 psi
ASTM D790
Flexural Modulus 0.841 GPa
122 ksi
Tangent; ASTM D790
Izod Impact, Notched NB
NB
73°F; ASTM D256
Gardner Impact 36.16 J
26.67 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 175 °C
347 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
Unannealed; ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 205 °C
401 °F
Middle Barrel Temperature 208 °C
406 °F
Front Barrel Temperature 213 °C
415 °F
Nozzle Temperature 213 °C
415 °F
Mold Temperature 13.0 - 47.8 °C
55.4 - 118 °F
Injection Pressure 2.41 - 8.27 MPa
350 - 1200 psi
Back Pressure 0.345 - 1.03 MPa
50.0 - 150 psi
Descriptive Properties Value Comments
Injection Rate Moderate-Fast
Users viewing this material also viewed the following: