Material Notes:
Al-27%Si controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 160 MPa
23200 psi
Tensile Strength, Yield 110 MPa
16000 psi
Modulus of Elasticity 80.0 GPa
11600 ksi
Flexural Strength 210 MPa
30500 psi
Three Point Bend
Thermal Properties Metric English Comments
CTE, linear 15.3 µm/m-°C

@Temperature 25.0 - 100 °C
8.50 µin/in-°F

@Temperature 77.0 - 212 °F
16.8 µm/m-°C

@Temperature 25.0 - 500 °C
9.33 µin/in-°F

@Temperature 77.0 - 932 °F
17.0 µm/m-°C

@Temperature 25.0 - 200 °C
9.44 µin/in-°F

@Temperature 77.0 - 392 °F
17.7 µm/m-°C

@Temperature 25.0 - 300 °C
9.83 µin/in-°F

@Temperature 77.0 - 572 °F
Specific Heat Capacity 0.8463 J/g-°C
0.2023 BTU/lb-°F
Thermal Conductivity 151.2 W/m-K

@Temperature 200 °C
1049 BTU-in/hr-ft²-°F

@Temperature 392 °F
177.4 W/m-K

@Temperature 25.0 °C
1231 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Component Elements Properties Metric English Comments
Aluminum, Al 73 %
73 %
Silicon, Si 27 %
27 %