| Category | Polymer , Thermoplastic , Elastomer, TPE |
| Manufacturer | Shin-Etsu Silicones |
| Trade Name | LIMS™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Shin-Etsu Silicones LIMSâ„¢ KEG2002-60A/B Elastomer.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | |
| Viscosity | 700000 cP | 700000 cP | A |
| 700000 cP | 700000 cP | B | |
| Linear Mold Shrinkage | 0.026 cm/cm | 0.026 in/in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 60 | 60 | |
| Tensile Strength | 10.0 MPa | 1450 psi | |
| Elongation at Yield | 410 % | 410 % | |
| 100% Modulus | 0.00267 GPa | 0.387 ksi | |
| Tear Strength | 42.0 kN/m | 240 pli | |
| Compression Set | 8.0 % <br>@Temperature 200 °C,<br> Time 14400 sec |
8.0 % <br>@Temperature 392 °F,<br> Time 4.00 hour |
|
| 34 % <br>@Temperature 150 °C,<br> Time 3600 sec |
34 % <br>@Temperature 302 °F,<br> Time 1.00 hour |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 5.00 min <br>@Temperature 150 °C |
0.0833 hour <br>@Temperature 302 °F |
Press Cure |
| 60.0 min <br>@Temperature 150 °C |
1.00 hour <br>@Temperature 302 °F |
Post Cure |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Translucent | |
| Cure Rate | 28 | T10 (302°F, ODR) |
| 40 | T90 (302°F, ODR) |