Material Notes:
Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 62-75Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Physical Properties Metric English Comments
Density 8.36 g/cc
0.302 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 68 - 90
68 - 90
Hardness, Vickers 121 - 185
121 - 185
Tensile Strength, Ultimate 510 - 610 MPa
74000 - 88500 psi
Tensile Strength, Yield 410 - 560 MPa
59500 - 81200 psi
Elongation at Break 20 - 45 %
20 - 45 %
Modulus of Elasticity 131 GPa
19000 ksi
Fatigue Strength 210 - 240 MPa

@# of Cycles 1.00e+8
30500 - 34800 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Thermal Properties Metric English Comments
CTE, linear 17.0 µm/m-°C

@Temperature 20.0 - 200 °C
9.44 µin/in-°F

@Temperature 68.0 - 392 °F
Thermal Conductivity 105 W/m-K
729 BTU-in/hr-ft²-°F
Melting Point 870 - 980 °C
1600 - 1800 °F
Solidus 870 °C
1600 °F
Liquidus 980 °C
1800 °F
Component Elements Properties Metric English Comments
Beryllium, Be 1.8 - 2.0 %
1.8 - 2.0 %
Co + Ni >= 0.20 %
>= 0.20 %
Co + Ni + Fe <= 0.60 %
<= 0.60 %
Copper, Cu 98 %
98 %
as balance
Lead, Pb <= 0.020 %
<= 0.020 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000910 - 0.0000115 ohm-cm
0.00000910 - 0.0000115 ohm-cm
15-19% IACS Conductivity