Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

M Cubed Technologies MMC-S55 Aluminum alloy-55% SiC Metal Matrix Composite

Category Metal , Metal Matrix Composite
Manufacturer M Cubed Technologies, Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M Cubed Technologies MMC-S55 Aluminum alloy-55% SiC Metal Matrix Composite.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High stiffness, low density composite. Parts are cast using several standard foundry techniques Size range varies from small components (1lb or smaller) to parts greater than 10 ft. square with complicated features, 1000-2000 lbs+. Applications in high-precision equipment: semiconductor, CMM, automotive, aerospace, and also in ballistic protection.Information provided by M Cubed Technologies, Inc.
Physical Properties Metric English Comments
Density 2.96 g/cc
0.107 lb/in³
ASTM C135
Mechanical Properties Metric English Comments
Modulus of Elasticity 200 GPa
29000 ksi
ASTM E494
Flexural Strength 340 MPa
49300 psi
ASTM C1161
Poissons Ratio 0.25
0.25
ASTM E494
Fracture Toughness 13.0 MPa-m½
11.8 ksi-in½
ASTM C1421
Shear Modulus 80.0 GPa
11600 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 11.8 µm/m-°C

@Temperature 25.0 - 100 °C
6.56 µin/in-°F

@Temperature 77.0 - 212 °F
ASTM E831
Thermal Conductivity 160 W/m-K
1110 BTU-in/hr-ft²-°F
ASTM E1461
Descriptive Properties Value Comments
Matrix Al Alloy
Particle Reinforcement SiC
Vol. % Reinforcement 55
Users viewing this material also viewed the following: