Material Notes:
Master Bond Polymer System EP79FL is a two component, silver-coated nickel, electrically conductive system for high performance bonding and sealing. Its most salient features are its high flexibility and elongation. EP79FL is highly flexible and is easier to remove than most silver-coated nickel epoxies, making it well suited for repair type applications.
Mechanical Properties Metric English Comments
Elongation at Break >= 60 %
>= 60 %
Adhesive Bond Strength >= 5.52 MPa
>= 800 psi
After 30 days water immersion
>= 5.86 MPa

@Temperature 23.0 °C
>= 850 psi

@Temperature 73.4 °F
Peel Strength >= 3.51 kN/m
>= 20.0 pli
Thermal Properties Metric English Comments
Thermal Conductivity 1.59 W/m-K
11.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -269 °C
-452 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.010 ohm-cm
<= 0.010 ohm-cm
Processing Properties Metric English Comments
Cure Time 120 - 180 min

@Temperature 65.6 °C
2.00 - 3.00 hour

@Temperature 150 °F
1440 - 2880 min

@Temperature 23.9 °C
24.0 - 48.0 hour

@Temperature 75.0 °F
Pot Life 60 - 75 min
60 - 75 min
100 gm mass
75 - 90 min
75 - 90 min
50 gm mass
Shelf Life 3.00 Month
3.00 Month
syringe
6.00 Month
6.00 Month
glass jar
Descriptive Properties Value Comments
Mixing Ratio (A to B) 1/1
Viscosity smooth paste