LyondellBasell SEQUEL® E3000 FR TPO

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO) , Polyolefin
Manufacturer LyondellBasell
Trade Name SEQUEL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell SEQUEL® E3000 FR TPO.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: SEQUEL® E3000FR thermoplastic olefinic elastomer (TPO) is designed for exterior and interior applications that require stiffness and durability. This extrusion-grade material is specially formulated to exhibit improved flame resistance. This material can be supplied with or without UV stabilizers. Applications: Sheet extrusion and thermoforming Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ASTM D955
Melt Flow 1.02 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.02 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Break 232 %
232 %
ASTM D638
Flexural Modulus 2.276 GPa
330.1 ksi
I.B., TAN, 0.5 in/min; ASTM D790
Izod Impact, Notched 8.28 J/cm
15.5 ft-lb/in
NB; ASTM D256
0.694 J/cm

@Temperature -30.0 °C
1.30 ft-lb/in

@Temperature -22.0 °F
HB; ASTM D256
Gardner Impact 33.4 J

@Temperature -30.0 °C
24.7 ft-lb

@Temperature -22.0 °F
ASTM D5420-96
>= 36.2 J

@Temperature 23.0 °C
>= 26.7 ft-lb

@Temperature 73.4 °F
ASTM D5420-96
Thermal Properties Metric English Comments
Flammability, UL94 V-1
V-1
all colors