Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Extrusion Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® PR92735 Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ApplicationsPETROTHENE PR 92735 is a high molecular weight, linear low density-based compound designed for cable jacketing. PR 92735 contains a nominal carbon black content of 2.6% and antioxidant has been added to ensure thermal stability during processing. PR 92735 also contains a processing aid.Processing TechniquesPR 92735, like other thermoplastic polyolefin compounds, can be extruded as wire and cable insulation using a conventional extruder. However, it has been found that a high shear mixing screw design improves the processability of this type of material. A typical drawdown ratio for this material is 3.17:1. Below are suggested extrusion conditions for PR 92735. These conditions are intended as general guidelines only and are not optimum values, since manufacturing conditions, such as extruder type and size, affect the processing of thermoplastic compounds.Industry SpecificationsPR 92735 meets the requirements of the following: ASTM D 1248, Type 1, Category 4, Class C, Grades E5, J1 and J3 Federal LP 390C, Type 111, Class L, Grades 2, 3, and 4, Category 4: REA PE 200, Appendix E.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D1505
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
Condition A - 10% Igepal®; ASTM D1693
Absorption Coefficient 440
440
ASTM D3349
Carbon Black Loading 2.6 %
2.6 %
Melt Flow 0.59 g/10 min
0.59 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
ASTM D224
Tensile Strength at Break 16.5 MPa
2400 psi
ASTM D638
Tensile Strength, Yield 11.0 MPa
1600 psi
ASTM D638
Elongation at Break 650 %
650 %
ASTM D638
Flexural Modulus 0.365 GPa
53.0 ksi
1% Secant; ASTM D790
1% Secant Modulus 248 MPa
36000 psi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 200 µm/m-°C

@Temperature 20.0 °C
111 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Brittleness Temperature <= -76.0 °C
<= -105 °F
F<sub>50</sub>; ASTM D746
Electrical Properties Metric English Comments
Dielectric Constant 2.5

@Frequency 1e+6 Hz
2.5

@Frequency 1e+6 Hz
ASTM D1531
Dielectric Strength 19.7 kV/mm
500 kV/in
ASTM D149
Dissipation Factor 0.00040

@Frequency 1e+6 Hz
0.00040

@Frequency 1e+6 Hz
ASTM D1531
Processing Properties Metric English Comments
Feed Temperature 154 - 163 °C
310 - 325 °F
Zone 2 177 - 193 °C
350 - 380 °F
Zone 3 193 - 210 °C
380 - 410 °F
Zone 4-x 204 - 218 °C
400 - 425 °F
Adapter Temperature 204 - 218 °C
400 - 425 °F
Die Temperature 204 - 218 °C
400 - 425 °F